Автора пока нетВзять себе
- Лицензия
- CC0 1.0 (общественное достояние)По материалам www.nist.gov
- Языки
- English
- Темы
- Наука
NIST scientists found a way to build a 3D optical image of a chip wafer quickly and without damaging it, which can reveal defects only nanometers across. Rick Silver and Bryan Barnes, of the Semiconductor and Dimensional Metrology Division, say it improves defect sensitivity by five-fold or more over 2D imaging.
The problem
As device features shrink beyond 22 nm, even a defect a few nanometers across can ruin a device and hurt a manufacturer's yield, and finding one on a 300 mm wafer is daunting. Silver offers an analogy: one foot in 3,000 miles equals a 10 nm defect over a 300 mm wafer. The International Technology Roadmap for Semiconductors lists inspection of defects in shrinking devices as lacking known solutions.
Companies use optics to quickly check a wafer for defects, then take it off the line to a scanning electron microscope (SEM) to identify the defect. Barnes says the SEM is excellent for high-resolution review but cannot cover the wafer fast enough, so optics are needed. The goal is a method that is quick, cheap and non-destructive on 300 mm and 450 mm wafers.
The method
The technique builds on scatterfield microscopy, invented at NIST. It lights the target from various angles with chosen combinations of transverse-magnetic and transverse-electric polarization, which sets up a three-dimensional interference field above the sample.
- Hardware. The work used a NIST-built 193 nm wavelength microscope, but the process can be repeated on any Köhler-illuminated microscope with fine focus control, so companies need not replace expensive equipment.
- Test sample. An intentional defect array from SEMATECH, designed to mimic inspection of circuits with nearly 9 nm linewidths, with bridge connection errors and line breaks.
- Steps. The scientists collected several images through best focus, correlated them in the x, y and z planes, and subtracted a reference volume from the defect volume. In-house software aligned and combined the slices into a 3D volume.

A defect as imaged by (a) SEM, (b) scatterfield optical microscopy and (c) simulation. Such a 2D optical image would be one focus slice in the 3D detection process for sub-10 nm defects. Image from NIST's page.

(a) Four focal slices stacked into a simulated 3D image; (b) the difference between reference data and the simulated defect; (c) simulated defect detection. Image from NIST's page.
Silver says independent focus slices make a volume in which nearest neighbors in all three dimensions can be used, which significantly enhances the information available.
What remains
The simulations show the ability to find defects smaller than industry currently needs. Silver says there is no question defects can be seen at 10 nm and guesses 6 nm is also doable. The open question is the complexity of the layer stack, since each layer adds variability and background signal.
Sources
- NIST Physical Measurement Laboratory, https://www.nist.gov/news-events/news/2013/05/new-3d-defect-detection-fills-important-industry-gap ; rewritten in hubnx's own words. The photo of NIST staff on the original page is left out.