When a transistor gate shrinks to about 12 nanometers, the electron microscope that measures it can mistake a change in shape for a change in width. NIST researchers have built a model-based way to tell the two apart, and tested it with Intel Corporation on next-generation samples.

The measuring problem

According to the International Technology Roadmap for Semiconductors, within a couple of years the typical length of a transistor’s gate, its on-off switch, would be under 20 nanometers (nm). Production tolerances at that size need measurements with a minimum uncertainty around 0.3 nm. By 2020 gate lengths were expected to fall to around 12.5 nm, which demands uncertainties near 0.2 nm, about the width of one silicon atom.

Chip makers usually find a feature’s critical dimensions by locating its edges with a scanning electron microscope (SEM). An SEM counts the low-energy electrons knocked out of a sample by a high-energy beam, and the counts peak at edges. Typical imaging uses approximation algorithms that place an edge within a possible range of one or two nanometers.

What NIST found

NIST researchers determined that, at the scale of the latest chips, SEM measurements are strongly affected by variations in a gate’s three-dimensional shape that arise in fabrication:

  • line width and center position;
  • the angle of a raised feature’s sidewalls;
  • the curvature radius of its top edge;
  • the effect of neighboring structures.

Each one changes the paths of the ejected electrons, so it is hard to locate edges and therefore the true width and shape. Process control generally does not allow for this. Fabricators compare one production run with another and assume differences come from real changes in the dimension plus random measurement error. NIST scientists say the differences may instead come from shape changes, some of them unrelated to the dimension in question. The lead author said the industry needs something that can handle arbitrary three-dimensional shapes, because a critical-dimension number that responds to both width and shape measures both in some poorly defined way.

Three-dimensional reconstruction of chip features from measurements using the NIST model-library method

A three-dimensional reconstruction of chip features from measurements made with the NIST model-library method. Image from NIST’s page.

The model library

NIST scientists modelled how electrons ejected from the gate travel during an SEM scan, given shape variations and instrument settings such as beam tilt, brightness, offset and beam size. They combined the physics of electron transit with detailed databases of electron transmission and scattering, using random numbers to simulate the probabilistic nature of scattering. They repeated this for each of 27,000 combinations of parameters. The result is a library of SEM signatures for different shape combinations. A measured signature can be compared with the library to infer the sample’s parameters accurately.

Shape variations caused by successive etching stages used to reduce feature size

Successive etching stages used to reduce feature size can cause considerable variation in shape and in pitch, the distance between the centers of two adjacent features. Image from NIST’s page.

Testing it

With Intel Corporation the team tested the method on special samples that Intel made at next-generation dimensions of 10 nm to 12 nm. In a publication in Ultramicroscopy, the collaborators report that width and shape results from the model library agreed with measurements of the same gates by two completely different high-accuracy technologies to better than 1 nm.

What is next

The lead author said no integrated circuit manufacturer used this kind of model-based metrology at the time, but might adopt it if SEM makers built the capability into their instruments, which could significantly raise the accuracy of current measurements. Reaching sub-nanometer uncertainties would need more accurate models, and those need measurements that NIST’s lab did not then have, such as absolute rather than relative yield, meaning how many electrons leave the sample per electron the SEM sends in. That would likely need custom instrumentation, at a time when the budget to maintain existing instruments was already a problem.

Sources

Комментарии

Spinner Logo

Ещё на тему «Наука»

Автор: Hub Nexus editors
Top 10 in AI, week of 2 November 2026
Автор: Hub Nexus editors
Top 10 in AI, week of 26 October 2026
Автор: Hub Nexus editors
Top 10 in AI, week of 19 October 2026
Автор: Hub Nexus editors
Top 10 in AI, week of 12 October 2026
CC0 1.0 (общественное достояние)
Sea ice grows throughout the winter and melts throughout the summer, reaching its maximum extent in late February or March, and its minimum extent in September. The ice that survives at least one summer melt season is typically thicker and more likely to survive future summers. Since the 1980s, the
CC0 1.0 (общественное достояние)
Alaska's Deep-Sea Sponges: Building a Library of Species Nobody Has Named Yet